PENGGUNAAN BATU KAPUR SEBAGAI PENGGANTI AGREGAT KASAR DITINJAU DARI KUAT TEKAN BETON

PRIMA, APRISYA DWI and SYAPUTRI, INDRIYANTI (2016) PENGGUNAAN BATU KAPUR SEBAGAI PENGGANTI AGREGAT KASAR DITINJAU DARI KUAT TEKAN BETON. Other thesis, POLITEKNIK NEGERI SRIWIJAYA.

[img]
Preview
Text
COVER.pdf

Download (270kB) | Preview
[img]
Preview
Text
BAB I.pdf

Download (207kB) | Preview
[img]
Preview
Text
BAB II.pdf

Download (357kB) | Preview
[img] Text (BAB III Metodologi Penelitian)
BAB III.pdf
Restricted to Repository staff only

Download (661kB)
[img] Text (BAB IV Pembahasan)
BAB IV.pdf
Restricted to Repository staff only

Download (923kB)
[img]
Preview
Text
BAB V.pdf

Download (161kB) | Preview
[img]
Preview
Text
DAFTAR PUSTAKA.pdf

Download (162kB) | Preview
[img] Text (Data Pengujian)
LAMPIRAN.pdf

Download (0B)

Abstract

Concrete which compose by hidraulic cement, coarse agregate, fine agregate, water with or without admixture or additive. The great of enhancement from the necessity of cocncrete constituent triggers rock mining as one of concrete constituent material. Which cause decreasement of the existing natural resource. These will effects the coarse aggregate necessity as one of concrete constituent material. To fullfill the necessity of low existing natural resource find the subtitude alternative which appropriated the standard . There is a limestone mining in Ogan Komering Ulu which dominated by limestone’s excavation. These becomes a reason the use of limestone to fullfill the concrete constituent material by people around. This research aims to find the increased or the Decreased percentage that will effect the compressive strength on the 28th day with the percentage compositions: 25%; 35%; 45%; 55%; 65%; and 75%. Based on the result of the compressive strength research in laboratory proves that the reduction of compressive strength on the 28th day: 28,065% for compotition 25% of lime stone with compressive strenght 125,332 kg/cm2; 27,812% for compotition 35% of lime stone with compressive strength 125,774 kg/cm2; 27,119% for compotition 45% of lime stone with compressive strength 126,841 kg/cm2; 27,267 % for compotition 55% of lime stone with compressive strength 126,722 kg/cm2. 27,434 % for compotition 65% of lime stone with compressive strength 126,431 kg/cm2. 28,207 % for compotition 75% of lime stone with compressive strength 125,085 kg/cm2.

Item Type: Thesis (Other)
Uncontrolled Keywords: Beton, Kuat tekan, Batu Kapur
Subjects: T Technology > TA Engineering (General). Civil engineering (General)
Divisions: Civil Engineering > Undergraduate Theses
Depositing User: Mrs Trisni Handayani
Date Deposited: 13 Oct 2017 02:51
Last Modified: 13 Oct 2017 02:51
URI: http://eprints.polsri.ac.id/id/eprint/4135

Actions (login required)

View Item View Item