PENGOLAHAN AIR GAMBUT MENGGUNAKAN MEMBRAN KOMPOSIT POLYSULFONE-POLYAMIDE (PSF-PA) SECARA MIKROFILTRASI

Jannatul, Fitri (2016) PENGOLAHAN AIR GAMBUT MENGGUNAKAN MEMBRAN KOMPOSIT POLYSULFONE-POLYAMIDE (PSF-PA) SECARA MIKROFILTRASI. Other thesis, Politeknik Negeri Sriwijaya.

[img]
Preview
Text (COVER)
HALAMAN DEPAN.pdf

Download (356kB) | Preview
[img]
Preview
Text (BAB 1 PENDAHULUAN)
BAB I.pdf

Download (139kB) | Preview
[img]
Preview
Text (BAB 2 LANDASAN TEORI)
BAB II.pdf

Download (537kB) | Preview
[img] Text (BAB 3 METODOLOGI PENELITIAN)
BAB III.pdf
Restricted to Repository staff only

Download (111kB)
[img] Text (BAB 4 HASIL DAN PEMBAHASAN)
BAB IV.pdf
Restricted to Repository staff only

Download (355kB)
[img]
Preview
Text (BAB 5 KESIMPULAN DAN SARAN)
BAB V.pdf

Download (89kB) | Preview
[img]
Preview
Text (DAFTAR PUSTAKA)
DAFTAR PUSTAKA.pdf

Download (90kB) | Preview

Abstract

PEAT WATER TREATMENT WITH COMPOSITE MEMBRANE POLYSULFONE-POLYAMIDE (PSF-PA) BY MIKROFILTRATION (Jannatul Fitri, 2016, 64 Pages, 8 Tables, 8 pictures, 4 Attachment) The purpose of this research in addition to get clean water is to dtermine the optimal conditions of varying concentrations of coagulant and operating pressure adn rejection coefficient of each parameter tested. This research used an experimental method, observation, tabulations adn regression graphically. The processing is done by affixing a coagulant alum, sedimentation and filtration are passed on polysulfone-polyamide composite membrane (PSF-PA). The parameters analyzed is pH, TDS, salinity and turbidity. The result showed that the optimum conditions of pH rejection is at a pressure of 2.5 bar with a concentration of 300 ppm coagulant which produces a pH value of 5.5 with rejection value reached 64.18%. The optimum conditions TDS rejection coefficient is at a concentration of 300 ppm and 0.5 bar pressure which produces 470 ppm TDS values with a rejection coefficient reached 60.07%. The optimum conditions of salinity rejection coefficient reached 63.55% at a pressure of 0.5 bar and a concentration of 300 ppm which produces the salinity value of 257 ppm. The optimum conditions of a rejection coefficient turbidity reached 90.49% were obtained at a pressure of 2.5 bar with the addition of 300 ppm of coagulant that returns a value of 9.7 NTU.

Item Type: Thesis (Other)
Uncontrolled Keywords: composite membrane, polysulfone-polyamide, rejection, peat water.
Subjects: T Technology > TP Chemical technology
Divisions: Chemical Engineering > Undergraduate Theses
Depositing User: Mr Bambang Anthony
Date Deposited: 09 Oct 2017 00:56
Last Modified: 09 Oct 2017 00:56
URI: http://eprints.polsri.ac.id/id/eprint/4112

Actions (login required)

View Item View Item