PATRICIA, NATASHIA CINDY (2016) PENGARUH VARIASI KOMPOSISI KITOSAN DANPLASTICIZER GLISEROL DALAM PEMBUATAN PLASTIK BIODEGRADABLE DARI PATI TALAS. Other thesis, POLITEKNIK NEGERI SRIWIJAYA.
|
Text
cover.pdf Download (415kB) | Preview |
|
|
Text (BAB I Pendahuluan)
BAB I.pdf Download (173kB) | Preview |
|
|
Text (BAB II Tinjauan Pustaka)
BAB II.pdf Download (657kB) | Preview |
|
![]() |
Text (BAB III Metodologi Penelitian)
BAB III.pdf Restricted to Repository staff only Download (364kB) |
|
![]() |
Text (BAB IV Hasil dan Pembahasan)
BAB IV.pdf Restricted to Repository staff only Download (662kB) |
|
|
Text (BAB V Kesimpulan dan Saran)
Bab V.pdf Download (146kB) | Preview |
|
|
Text
daftar pustaka.pdf Download (251kB) | Preview |
Abstract
Plastic waste including one of the problem of environment that most concern in Indonesia, even thought to have reached thousands of tons. Plastic will be breaks down in time 450 until 600 years. Therefor, needed plastic environmentally friendly to reduce pollution, for example biodegradable plastic.Biodegradable plastic are a type of plastic made from renewable biomass sources, such as vegetable oil, starch, and microbiota. Taro tuber starch can be used as raw material for the making of biodegradable plastics because taro tuber starch containing 74,34% carbohydrates. In this research , the making of biodegradable plastics using the casting method with variation of chitosan ( 0gr ; 0,5gr ; 1 g ) and glycerol volume variation ( 2ml , 3ml , 4ml )through 3 stages of that is making taro starch, making plastics and analysis of biodegradable plastic (tensile strenght, water resistance, a melting point and biodegradability test). The effect of adding glycerol volume will increase degradation time of plastic but reduce the value of tensile strength , water resistance % and a melting point. Effect of chitosan will increase the value of tensile strength and % water resistance , but it can decreasing degradation time of plastic. The best composition of biodegradable plastics in the research of plastic with 2ml of glycerol and 1gr chitosan that produce value 0,00226Mpa tensile strength ; % Water resistance of 64.79 % ; melting point 272.6 ; and biodegradation time for 5 days.
Item Type: | Thesis (Other) |
---|---|
Uncontrolled Keywords: | Plastik, Plastik biodegradable, Patitalas, Gliserol, Kitosan |
Subjects: | T Technology > TP Chemical technology |
Divisions: | Chemical Engineering > Undergraduate Theses |
Depositing User: | Mrs Trisni Handayani |
Date Deposited: | 28 Feb 2017 02:25 |
Last Modified: | 28 Feb 2017 02:25 |
URI: | http://eprints.polsri.ac.id/id/eprint/3315 |
Actions (login required)
![]() |
View Item |